Heat Shrinkable Medium Wall Insulating Tubing

zoom view

Features

  • CIMT is made from cross linked polyolefin
  • Medium wall
  • Excellent chemical & electrical properties
  • High Tensile strength
  • Non-corrosive
  • UV-resistant, Excellent environmental protection
  • Operating temperature: -55°C to 125°C
  • Standard Colour : Black, Red

Dimensions

Code (D)
Internal Diameter
(As Supplied)
(d)
Internal Diameter
(After Recovery)
Wall Thickness
(After Recovery)
CIMT -25/6 25 6 2.9-3.1
CIMT -33/8 33 8 2.9-3.1
CIMT -40/12 40 12 2.9-3.1
CIMT -55/16 55 16 2.9-3.1
CIMT -65/19 65 19 3.0-3.1
CIMT -75/22 75 22 3.0-3.1
CIMT -85/25 85 25 3.1-3.4
CIMT -95/25 95 25 3.1-3.4
CIMT -115/34 115 34 3.2-3.5
CIMT -140/42 140 42 3.3-3.6
CIMT -160/50 160 50 3.3-3.6
CIMT -180/58 180 58 3.4-3.7
CIMT -200/65 200 65 3.4-3.7

*All dimensions are in mm

Technical Properties

Property Requirements Test Method
Tensile strength ≥ 13.5 MPa ASTM D 2671
Tensile strength after aging (120°C/168 Hrs) ≥ 10 MPa ASTM D 2671
Longitudinal shrinkage 0 to -10% ASTM D 2671
Elongation at break ≥ 400% ASTM D 2671
Elongation at break after aging (120°C/168 Hrs) ≥ 250% ASTM D 2671
Dielectric Strength ≥20Kv/mm IEC 243
Dielectric constant 4.0 IEC 250
Volume resistance 1013 Ohm cm min. IEC 93
Flammability (oxygen index) ≥ 25 ASTM 4589
Copper corrosion (120°C/168Hrs) No corrosion ASTM D 2671
Cold bend (-40°C/4 Hrs) No corrosion ASTM D 2671
Water absorption (23°C/14 days) <0.5% ISO 62